[1]谢佳雨,施梦汝,谢伟丽. 两种粘接系统下树脂水门汀厚度对纤维桩粘接强度的影响[J].中国美容医学,2018,(05):73-76.
 XIE Jia-yu,SHI Meng-ru,XIE Wei-li. Effect of Resin Cement Thickness on Bonding Strength of Fiber Post under Two Kinds of Bonding System[J].Medical Aesthetics and Beauty,2018,(05):73-76.
点击复制

 两种粘接系统下树脂水门汀厚度对纤维桩粘接强度的影响
()
分享到:

《中国美容医学》[ISSN:1008-6445/CN:61-1347/R]

卷:
期数:
2018年05期
页码:
73-76
栏目:
出版日期:
2018-06-10

文章信息/Info

Title:
 Effect of Resin Cement Thickness on Bonding Strength of Fiber Post under Two Kinds of Bonding System
文章编号:
1008-6455(2018)05-0073-04
作者:
 谢佳雨施梦汝谢伟丽
Author(s):
XIE Jia-yu SHI Meng-ruXIE Wei-li
关键词:
 [关键词]粘接系统粘接强度树脂水门汀厚度纤维桩
Keywords:
 Key words: adhesive system bonding strength the thickness of resin cement fiber post
分类号:
R783.4
文献标志码:
A
摘要:
[摘要]目的:评估在全酸蚀和自酸蚀两种不同粘接系统下,不同厚度的树脂水门汀对纤维桩粘接性能的影响,为纤维桩在临
床操作过程中的应用提供理论依据。方法:将40颗因正畸拔除的单根管前磨牙经完善的根管治疗后随机的分为全酸蚀组(A
组)和自酸蚀组(B组)两组。每组再分别按1.2mm(1组),1.4mm(2组),1.6mm(3组),1.8mm(4组)的直径平均分为
四个小组进行桩道预备。分别记为A1,B1,A2,B2,A3,B3,A4,B4组。用通用型树脂粘接剂和双固化树脂水门汀将直径为
1.1mm的纤维桩与预备好的实验牙进行粘接。片切成厚度为1.5mm的试件,通过扫描电子显微镜对试件表面及材料粘接处进行
观察,利用薄片推出实验测试粘接强度,测试完成后在20倍体视显微镜下观察试件的破坏模式。结果:全酸蚀1.4mm组(A2
组)的粘接强度最高,自酸蚀1.8mm组(B4组)的粘接强度最低(P <0.05);两组试件中牙本质与树脂水门汀之间的破坏模式
(DR破坏模式)为主要的破坏模式。结论:树脂水门汀应用全酸蚀技术时粘接强度优于应用自酸蚀技术,且随着树脂水门汀
的厚度增加粘接强度先增强后降低,总体呈现下降趋势。

Abstract:

(Department of Prosthodontics, College of Stomatology, Harbin Medical University,Harbin 150000, Heilongjiang, China)
Abstract: Objective To evaluate the effect of different thickness of resin cements on the bonding properties of fiber post under
the two different bonding systems of total-etching and self-etching, and to provide theoretical basis for the application of fiber
post in the clinical operation process. Methods The 40 anterior molars with orthodontic extraction were randomly divided
into two groups after being treated with a perfect root canal, named the total Acid etching Group (Group A) and the self-acid
etching group (Group B). Each group was then pressed 1.2 mm (1), 1.4 mm (2), 1.6 mm (3), 1.8 mm (4) was divided into four
groups to prepare the post path. Recorded as A1, B1, A2, B2, A3, B3, A4, B4 Group. Using a universal adhesive and a dual
cured resin cement, bonded the diameter is 1.1mm fiber posts with the prepared experimental teeth. Slice cut to thickness of
1.5 mm specimens, By scanning electron microscope (SEM), the surface of the specimen and the bonding place of the material
were observed, Use the micro push-out test results of its bonding strength, The failure mode of the specimen was observed
under a 20-ploidy microscope after the completion of the test. Results Total-etching1.4 mm group(A2) has the highest bonding
strength, self-etching1.8 mm group (B4) has the lowest bonding strength(P <0.05);In the two groups of specimens, the failure
mode between dentin and resin cement was the main failure mode. Conclusion The adhesive strength of resin cement with
total acid etching technology is better than that with self-acid etching technology, and with the increase of the thickness of resin
cement, the bonding strength increases first and then decreases, and the overall downward trend is shown.

相似文献/References:

[1]. 埋线美容专栏[J].中国美容医学,2018,(01):0.
 [J].Medical Aesthetics and Beauty,2018,(05):0.
[2]杨 震. 应用透明质酸颏部填充联合A型肉毒毒素咬肌注射重塑面部下1/3轮廓的效果观察[J].中国美容医学,2018,(03):1.
 YANG Zhen. Effect of Hyaluronic Acid Chin Filling Combined with Botulinum Toxin Type A Masseter Muscle Injection to Reconstruct the Facial Contour of the Lower 1/3[J].Medical Aesthetics and Beauty,2018,(05):1.
[3]祝闽辉,张栋梁,叶祥柏,等. 皮肤软组织扩张术埋置注液期并发症危险因素研究[J].中国美容医学,2018,(03):4.
 ZHU Min-hui,ZHANG Dong-liang,YE Xiang-bo,et al. Risk Factors of Complications after Tissue Expasion[J].Medical Aesthetics and Beauty,2018,(05):4.
[4]刘申松,杨永成. 自体脂肪颗粒移植联合假体隆乳术在哺乳后乳腺萎缩整形术中的应用[J].中国美容医学,2018,(03):9.
 LIU Shen-song,YANG Yong-cheng. Application of Autologous Fat Granule Graft Combined with Prosthesis Combined Augmentation Mammoplasty in Breast Reconstruction of Breast Atrophy Patients after Breast-feeding[J].Medical Aesthetics and Beauty,2018,(05):9.
[5]韩 星,胡守舵,陈晓芳,等.自体脂肪颗粒移植促进手部年轻化的临床观察[J].中国美容医学,2018,(03):12.
 HAN Xing,HU Shou-duo,CHEN Xiao-fang,et al. The Effect of Autologous Fat Grafting in Hand Rejuvenation[J].Medical Aesthetics and Beauty,2018,(05):12.
[6]李胜旭,苏映军,杨 宽,等. 封闭负压引流技术在先天性并指分指植皮术中的应用[J].中国美容医学,2018,(03):15.
 LI Sheng-xu,SU Ying-jun,YANG Kuan,et al. Application of Vacuum Sealing Drainage for Skin Graft in Patients with Congenital Syndactyly of the Hand[J].Medical Aesthetics and Beauty,2018,(05):15.
[7]陈 波,路 会,马 力,等. 钝针皮下层扇形注射透明质酸矫正面颊部凹陷[J].中国美容医学,2018,(03):18.
 CHEN Bo,LU Hui,MA Li,et al. Correction of Cheek Depression by Fanshaped Hyaluronic Acid Injection in Subcutaneous Layers with Blunt Needle[J].Medical Aesthetics and Beauty,2018,(05):18.
[8]曾德斌,栗鹏程,邱勋永,等. 不同超薄游离穿支皮瓣修复手部软组织缺损效果比较[J].中国美容医学,2018,(03):21.
 ZENG De-bin,LI Peng-cheng,QIU Xun-yong,et al. Comparison on the Repair Effect of Different Ultrathin Free Perforator Flaps in the Treatment of Patients with Soft Tissue Defect of Hand[J].Medical Aesthetics and Beauty,2018,(05):21.
[9]程 定,崔树英,郑 乐,等. 改道引流联合VSD技术修复会阴部撕裂伤的临床研究[J].中国美容医学,2018,(03):24.
 CHENG Ding,CUI Shu-ying,ZHENG Le,et al. Clinical Study on Diverted Drainage Combined with Vacuum Sealing Drainage Technique to Repair the Laceration of the Perineum[J].Medical Aesthetics and Beauty,2018,(05):24.
[10]李云峰,吴泽勇,黄海华,等. 全厚皮片游离移植矫治儿童足背瘢痕挛缩畸形[J].中国美容医学,2018,(03):27.
 LI Yun-feng,WU Ze-yong,HUANG Hai-hua,et al. Full-thickness Skin Graft for the Treatment of Cicatricial Contracture of the Dorsum of Foot in Children[J].Medical Aesthetics and Beauty,2018,(05):27.

更新日期/Last Update: 2018-07-12