[1]陈健茵,范红燕.可见光固化树脂在前牙冠折再粘接修复中的应用[J].中国美容医学,2022,(6):138-141.
 CHEN Jianyin,FAN Hongyan.Application of Visible Light Curing Resin on Rebonding Repair of Anterior Crown Fracture[J].Medical Aesthetics and Beauty,2022,(6):138-141.
点击复制

可见光固化树脂在前牙冠折再粘接修复中的应用()
分享到:

《中国美容医学》[ISSN:1008-6445/CN:61-1347/R]

卷:
期数:
2022年6期
页码:
138-141
栏目:
出版日期:
2022-06-10

文章信息/Info

Title:
Application of Visible Light Curing Resin on Rebonding Repair of Anterior Crown Fracture
文章编号:
1008-6455(2022)06-0138-04
作者:
陈健茵范红燕
(湘南学院附属医院口腔科 湖南 郴州 423000)
Author(s):
CHEN JianyinFAN Hongyan
(Department of Stomatology,Affi liated Hospital of Xiangnan University, Chenzhou 423000,Hunan,China)
关键词:
牙折前牙冠折可见光固化复合树脂焦虑牙齿美观度
Keywords:
tooth fold anterior crown fracture visible light curing composite resin anxiety tooth aesthetics
分类号:
R783.3
文献标志码:
A
摘要:
目的:探讨可见光固化复合树脂(Light-cured composite, LCC)在前牙冠折再粘接修复中的美学效果及对患者 牙齿美观度的影响。方法:选取2014年1月-2019年1月笔者医院收治的80例前牙冠折患者,随机分为研究组(42例,采用 LCC材料修复)和对照组(38例,采用玻璃离子水门汀材料修复)。对比两组患者修复前与修复后1个月焦虑(Hamilton anxiety scale,HAMA)、抑郁(Hamilton depression scale,HAMD)评分,修复后12个月红/白美学指数(PES、WES) 及修复后24个月的并发症。结果:修复前,研究组HAMD、HAMA评分[(32.14±4.39)分、(22.16±4.29)分]与对照组 [(32.83±4.11)分、(21.58±4.15)分]对比,差异无统计学意义(t=0.382、0.721,P>0.05);修复后1个月,研究组 HAMD、HAMA评分[(18.59±2.61)分、(7.53±1.69)分]低于对照组[(25.27±3.59)分、(15.49±2.18)分],差异有统计 学意义(t=11.162、14.173,P<0.05);修复后12个月,研究组PES、WES各项得分均高于对照组,差异有统计学意义(P <0.05);修复后12个月、24个月研究组总并发症率4.76%、9.52%均低于对照组21.05%、34.21%,差异均有统计学意义 (χ2 =4.841、5.865,P<0.05)。结论:采用LCC材料对前牙冠折患者患牙进行再粘接修复的应用效果良好,可有效减轻患 者抑郁与焦虑情绪,提高修复后牙齿美观度并降低并发症发生率。
Abstract:
Objective To investigate the aesthetic eff ect of visible light cured composite resin (LCC) in the restoration of anterior crown fracture and its infl uence on the aesthetic degree of patients. Methods 80 patients with crown fracture of anterior teeth in our hospital from January 2014 to January 2019 were randomly divided into study group (42 cases, repaired with LCC material) and control group (38 cases, repaired with glass ionomer cement). HAMA and HAMD scores before and 1 month after repair, PES and Wes scores 12 months after repair, and complications 24 months after repair were compared between the two groups. Results The HAMD and HAMA scores of the study group before repair were (32.14±4.39) points,(22.16±4.29) points and control group (32.83±4.11) points, (21.58±4.15) points. There was no signifi cant diff erence between the two groups (t=0.382, 0.721, P>0.05).(18.59±2.61) points,(7.53±1.69)points was lower than that of the control group(25.27±3.59) points,(15.49±2.18)points. The difference was statistically significant (t=11.162,14.173,P<0.05); 12 months after repair, the PES and WES scores of the study group were higher than those of the control group, and the diff erence was statistically signifi cant (P<0.05); 12 months and 24 months after repair, the total complication rates of the study group were 4.76% and 9.52%, which were lower than 21.05% and 34.21% of the control group (χ2 = 4.841 and 5.865,P<0.05). Conclusion LCC is eff ective in the application of the reconnection and repair of the teeth in patients with anterior crown fracture, which can eff ectively reduce the depression and anxiety of the patients, improve the aesthetic degree of the teeth after the restoration and reduce the incidence of complications.

相似文献/References:

[1]蒋永福,朱 静,陈 栋. Ceramage聚合瓷在前牙冠折美容修复中的疗效及对牙体抗力的影响[J].中国美容医学,2019,(02):120.
 JIANG Yong-fu,ZHU Jing,CHEN Dong. Ceramic Age Ceramic Ceramics Can be Used to Repair the Effect of the AnteriorCrown and the Effect on the Tooth Resistance[J].Medical Aesthetics and Beauty,2019,(6):120.

更新日期/Last Update: 2022-07-05